Steel structure fireproof paint is an item that investors are interested in because of its high precaution against all problems that limit factory safety during production activities. Flame retardant paint with temperature sensor feature then automatically increases the thickness of the paint film to many times to create a wall to prevent the heat from contacting the iron and steel surface.
It is a kind of material that helps in saving and effective fire prevention. Fire retardant paint is composed of acrylic husk or epoxy compound and chemical additives. After being coated on the surface of the material that needs to be flame retardant, the fire retardant paint forms a protective layer to help the steel structure avoid unwanted effects such as fire, withstand temperature longer when fire and explosion occurs, and prolong the life of the steel structure. time for the fire brigade to arrive in time.

Flame retardant paint produces fish when it is non-flammable and non-toxic, helping to maintain structural steel temperatures below 400 degrees. Make sure the workshop frame stands firmly for up to 2-3 hours in the event of a fire.
Inflammation mechanism when encountering fire, the maximum expansion is 80 times higher than the original at a temperature of 150 degrees, the first paint produces Phoshoric Acid gas. At temperatures below 300, the paint opens into an insulating layer and creates fire-blocking gases. Below 500 degrees, the process of anti-carbonization causes the paint to begin to expand and soften into a gppm layer. Below 100 degrees, the paint expands to the point of stoois to retain CO2 and prevent the impact of fire on the steel structure.
The construction of steel structure fire retardant paint is not easy because it requires many layers of paint to be applied to the surface of the steel structure.
The application process of this paint requires strict compliance and high technique.
Step 1: Surface treatment of metal steel frame
Step 2: Spray a suitable anti-rust paint
Step 3: Finish coating with fireproof paint
Step 4: Finish the color coating
Step 5: Conduct acceptance test of the project.